氫氧化鉀粘結(jié)的原因以及解決方法

發(fā)布來源:http://www.fahao168.com    更新時間:2022-11-10 點(diǎn)擊數(shù):117

如果氫氧化鉀長時間不使用,如果我們不能保證其儲存環(huán)境,就會造成受影響的產(chǎn)品受到濕度的影響。此外空氣中的氧氣和水也容易造成氫氧化鉀粘結(jié)問題。氫氧化鉀一旦粘結(jié)以后使用效果會打折扣。所以我們在使用的時候要注意操作的保護(hù),下面我們來了解一下氫氧化鉀粘結(jié)的原因以及解決方法。
If potassium hydroxide is not used for a long time, if we cannot guarantee its storage environment, the affected products will be affected by humidity. In addition, oxygen and water in the air are also easy to cause the sticking problem of potassium hydroxide. The use effect of potassium hydroxide will be reduced once it is bonded. Therefore, we should pay attention to the protection of the operation when we use it. Now let's learn about the causes of potassium hydroxide sticking and the solutions.
1.吸濕結(jié)塊。
1. Moisture absorption and agglomeration.
雙層包裝袋用于氫氧化鉀包裝。如果接縫不夠快或不夠緊,氫氧化鉀很容易吸收包裝袋中的水分,影響其質(zhì)量。因此將原來的單縫改為雙縫,要求包裝人員檢查夾緊、縫紉等工藝。很大程度上隔絕了空氣,大大減少了結(jié)塊導(dǎo)致密封松動的發(fā)生。
Double layer packaging bag is used for potassium hydroxide packaging. If the joint is not fast or tight enough, potassium hydroxide will easily absorb the moisture in the packaging bag and affect its quality. Therefore, the original single seam is changed to double seam, and the packaging personnel are required to check the clamping, sewing and other processes. The air is largely isolated, and the occurrence of seal looseness caused by caking is greatly reduced.
氫氧化鉀
2.受溫度影響。
2. Affected by temperature.
氫氧化鉀的溫度由滾筒的冷卻水流速和滾筒的轉(zhuǎn)速決定。循環(huán)水量、循環(huán)水溫度、料筒內(nèi)噴嘴是否堵塞、料筒是否結(jié)垢直接影響產(chǎn)品溫度,嚴(yán)重影響機(jī)械下料溫度的均勻性。清洗噴嘴后,清洗桶內(nèi)水垢,增加循環(huán)水量。將氫氧化鉀溫度從63c-66c降58C。通過降低下料溫度,可以減少結(jié)塊現(xiàn)象。
The temperature of potassium hydroxide is determined by the cooling water flow rate of the drum and the rotating speed of the drum. The circulating water volume, circulating water temperature, whether the nozzle in the barrel is blocked, and whether the barrel is scaling directly affect the product temperature, and seriously affect the uniformity of the mechanical blanking temperature. After cleaning the nozzle, clean the scale in the bucket and increase the circulating water volume. Reduce the temperature of potassium hydroxide from 63c-66c to 58C. By lowering the blanking temperature, agglomeration can be reduced.
氫氧化鉀粘結(jié)的原因很多,與環(huán)境和溫度的關(guān)系很大,要特別注意這兩個方面。為了避免影響我們的使用,它的日常保護(hù)和儲存要考慮很多因素,每個環(huán)節(jié)都不要草率。畢竟它的質(zhì)量也是影響使用效率的基本因素之一。
There are many reasons for the sticking of potassium hydroxide, which is closely related to the environment and temperature. Special attention should be paid to these two aspects. In order to avoid affecting our use, many factors should be taken into consideration in its daily protection and storage, and each link should not be hasty. After all, its quality is also one of the basic factors affecting the use efficiency.
氫氧化鉀儲存在陰涼、干燥、通風(fēng)良好的倉庫中。遠(yuǎn)離火種和熱源。倉庫內(nèi)的濕度不應(yīng)超過85%。氫氧化鉀包裝須密封并防潮。它應(yīng)與可燃材料和酸分開儲存,不應(yīng)混合。儲存區(qū)應(yīng)配備合適的材料以防止泄漏。更多相關(guān)產(chǎn)品的注意事項(xiàng)就來我們網(wǎng)站http://www.fahao168.com進(jìn)行咨詢吧!
Potassium hydroxide is stored in a cool, dry and well ventilated warehouse. Keep away from kindling and heat sources. The humidity in the warehouse shall not exceed 85%. The potassium hydroxide package must be sealed and moisture resistant. It shall be stored separately from combustible materials and acids and shall not be mixed. The storage area shall be equipped with suitable materials to prevent leakage. More precautions for related products can be found on our website http://www.fahao168.com Consult!

聯(lián)系我們

濟(jì)南金昊化工有限公司

電話:13869119097

傳真:0531-88529097

售后:0531-88529097

地址:濟(jì)南市天橋區(qū)桑梓店鎮(zhèn)化工市場南區(qū)

掃描二維碼,關(guān)注我們

13869119097

全國客戶服務(wù)熱線

濟(jì)南金昊化工有限公司

備案號:魯ICP備19046505號-2